Q420FTE鋼板舞陽鋼廠供應Q420FTE鋼板現貨庫存Q420FTE鋼板價格
Q420FTE鋼板化學成分:
牌號 |
C |
Mn |
P |
S |
Si |
Nb |
V |
Ti |
Mo |
Cr |
Ni |
Cu |
Al |
N |
Q420FTC |
≤0.20 |
1.00-1.70 |
≤0.025 |
≤0.015 |
≤0.50 |
≤0.060 |
≤0.15 |
≤0.050 |
≤0.20 |
≤0.30 |
≤0.50 |
≤0.30 |
≥0.015 |
≤0.012 |
Q420FTD |
≤0.20 |
1.00-1.70 |
≤0.025 |
≤0.015 |
≤0.50 |
≤0.060 |
≤0.15 |
≤0.050 |
≤0.20 |
≤0.30 |
≤0.50 |
≤0.30 |
≥0.015 |
≤0.012 |
Q420FTE |
≤0.20 |
1.00-1.70 |
≤0.020 |
≤0.010 |
≤0.50 |
≤0.060 |
≤0.15 |
≤0.050 |
≤0.20 |
≤0.30 |
≤0.50 |
≤0.30 |
≥0.015 |
≤0.010 |
Q420FTF |
≤0.20 |
1.00-1.70 |
≤0.020 |
≤0.010 |
≤0.50 |
≤0.060 |
≤0.15 |
≤0.050 |
≤0.20 |
≤0.30 |
≤0.50 |
≤0.30 |
≥0.015 |
≤0.010 |
成分備注:應至少加入細化晶粒元素Al、Nb、V、Ti其中一種,可單獨加入或以任一組合加入,并保證其中至少有一種含量≥0.015,混合加入時,總量≤0.22;可用Alt代替Als,此時Alt≥0.02;如果添加其他固N元素,酸溶鋁(Als)和全鋁(Alt)含量不適用。Ceq = C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15 Pcm=C+Si/30+(Mn+Cu+Cr)/20+Ni/60+Mo/15+V/10+5B
Q420FTE鋼板力學性能:
牌號 |
橫向下屈服強度MPa≥ |
抗拉強度Mpa |
斷后伸長率A% |
沖擊吸收能量J ≥ |
180°彎曲試驗 d-彎心直徑,a=試樣厚度 |
|||
鋼板厚度/mm |
鋼板厚度/mm |
|||||||
≤16 |
16-40 |
40-100 |
≤16 |
16-100 |
||||
Q420FTC、Q420FTD |
420 |
400 |
390 |
520-680 |
19 |
47 |
d=2a |
d=3a |
Q420FTE、Q420FTF |
420 |
400 |
390 |
520-680 |
19 |
34 |
d=2a |
d=3a |
Q420FTE鋼板尺寸、外形、重量及允許偏差:
鋼板的尺寸、外形、重量及允許偏差應符合GB/T709的規定。
牌號 | 厚度 | 寬 | 長 | 鋼廠 |
Q420FTE | 8 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 10 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 12 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 14 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 16 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 18 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 20 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 22 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 24 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 26 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 28 | 2200/2500 | 10000/12000 | 舞鋼 |
Q420FTE | 30 | 2200 | 11000 | 舞鋼 |
Q420FTE | 32 | 2200 | 11000 | 舞鋼 |
Q420FTE | 34 | 2200 | 11000 | 舞鋼 |
Q420FTE | 36 | 2200 | 11000 | 舞鋼 |
Q420FTE | 40 | 2200 | 11000 | 舞鋼 |
Q420FTE | 45 | 2200 | 11000 | 舞鋼 |
舞鋼188-3825-3183 |