S 114
C2.5 Cr30 W12Co Rem.
HRc≥53. Wear and heat resistance at high temperature, bad shock resistance. Hardfacing of three-cone bit.HRc≥53,高溫下耐磨、耐熱,但抗沖擊較差。堆焊牙輪鉆頭